    Everybody knows that its hard to beat the price of stuff at HF. Some of the stuff is better than others.

    I got a roller stand for wood working. The base assembly is very poorly done. The first time I used it, it fell apart. I've had spotty success with it as it seems to work only about 1/2 the time.

    Given that it wasn't all that great, I figured I didn't have a lot to lose if I wrecked in in trying to improve it.

    So, I ground the paint off and welded the base to the legs.

    Click image for larger version. 

Name:	IMG_4213.jpg 
Views:	441 
Size:	145.4 KB 
ID:	3692

    It was really had to get a good ground. I had to put the ground clamp on the opposite side of the leg I was welding. The other thing that was interesting is that the paint near where I was welding would catch on fire. It would go out fast, but I'm sure the fumes weren't good.

    I'd say the fix was a success as I know that I can use it now without it falling apart.
    Just starting in Aug '10
    ---
    Hobart Handler 187
    Power Plasma 50

  2. #2

    Default

    I had a similar issue with a HF roller seat (they don't sell it anymore, and the one they have now doesn't have a good tray)

    Just don't get any of those flames near your Hovercraft project, I'm not so sure they will go out as fast....
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3

    Default

    What caused it to fall apart ? I have four HF roller stands I use with my cabinet saw and band saw, they all feel solid... no problems at all.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    Quote Originally Posted by zoama585 View Post
    What caused it to fall apart ? I have four HF roller stands I use with my cabinet saw and band saw, they all feel solid... no problems at all.
    The base tube attaches to the leg using a hex head machine screw that goes up from the bottom of the base tube to a small threaded rod that slides into a hole in the leg. (If you've seen it, it should make sense.)

    The rod in the leg is barely bigger than the width of the leg, so any lateral motion causes the rod to slide half way out.
    Just starting in Aug '10
    ---
    Hobart Handler 187
    Power Plasma 50

  5. #5

    Default

    Quote Originally Posted by EmptyNester View Post
    The base tube attaches to the leg using a hex head machine screw that goes up from the bottom of the base tube to a small threaded rod that slides into a hole in the leg. (If you've seen it, it should make sense.)

    The rod in the leg is barely bigger than the width of the leg, so any lateral motion causes the rod to slide half way out.
    I thought that would be a problem when I assembled mine but it hasn't yet. Maybe I haven't put as much weight on mine... yet.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Project #5 from EmptyNester - Thrust Duct Support for Hovercraft
    By EmptyNester in forum Hobyist Projects
    Replies: 5
    Last Post: 10-25-2011, 02:24 AM
  2. Project #3 from EmptyNester - Hovercraft Control Stick
    By EmptyNester in forum Hobyist Projects
    Replies: 2
    Last Post: 10-16-2011, 10:30 PM
  3. Project #1 from EmptyNester - Welding cart (continued)
    By EmptyNester in forum Other Custom Fabrications
    Replies: 0
    Last Post: 10-16-2011, 09:32 PM
  4. Project #2 from EmptyNester
    By EmptyNester in forum Other Custom Fabrications
    Replies: 0
    Last Post: 10-09-2011, 06:11 PM
  5. bead roller work (Pictures)
    By Ram48 in forum Personal Projects (no welder required)
    Replies: 7
    Last Post: 05-11-2011, 02:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •