I wonder if you could improve your rust removal 'cell' by cutting the bottom out of a gladware containter that's the same size as the sponge and hot-gluing some soft rubber around the bottom. you should be able to get the sponge more saturated that if it were just sitting in open air. the more solution, the higher the electron mobility will be and the faster it will work.