Share
Results 1 to 4 of 4

Thread: Add Mig to a PP 256

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Add Mig to a PP 256

    Hey all i love my PP256 to death done alot of work with it so far, i recently bought a new home and i have taken on the roll of welder/ fabricator in my neighbor hood. Who is to complain about free beer and some cash on the side right? My question as in the title is simple i have been doing some welding for some of my neighbors that i find easier done with a mig, welding handles on lawn mowers and such, i dont mind tig'ing them but it would be nice to not have to prep so much for simple stuff. Is there a way to add a spool gun or something similar, maybe use a dead wire feed and power it using my pp256, in order to add wire feed to this awsome machine? Im looking more for someone that has done it then just theory, but i will be happy with any advice.

    Thanks!!

  2. #2

    Default

    We answer this all the time here on the forum. In short NO. Google Constant Current versus Constant Voltage, and you'll see why.

  3. #3
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    It can work with something like a Miller Suitcase X-Treme 12VS set to CC mode but it will not work well and for what the Miller cost you could buy a mig.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  4. Default

    Thanks guys i did some reading up on it before and after i posted, i just wasnt sure if anyone had any luck with it.