    Did you just throw a weld on the surface of the case? If so, I'm not so sure that is going to survive the vibration of a Shovelhead :-)
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  2. #2

    Default

    man that was one nasty crack. like sportbike said, i hope it holds up. how much more time did you spend fixing the "bent" casae?
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  3. #3
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    Quote Originally Posted by jerky View Post
    man that was one nasty crack. like sportbike said, i hope it holds up. how much more time did you spend fixing the "bent" casae?
    My STUPIDITY, all said and told, cost me a total of about 7-8 hours, if you count the time spent inventing new swear-words to express my frustration with
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

Similar Threads

  1. Project 1 From Hooda Tranny case repair (FOR 1st 2013)
    By hooda in forum On Road Fabrication
    Replies: 19
    Last Post: 01-22-2013, 06:23 AM
  2. Regulator rebuild
    By DaveO in forum Personal Projects (no welder required)
    Replies: 0
    Last Post: 01-02-2013, 12:11 AM
  3. Carburetor rebuild project.
    By Brian Ski in forum Personal Projects (no welder required)
    Replies: 9
    Last Post: 03-25-2012, 01:52 PM
  4. Project# 1 Weld Table
    By brianscott in forum Other Custom Fabrications
    Replies: 5
    Last Post: 01-19-2012, 02:53 PM
  5. One-off Harley fender project #1
    By hooda in forum On Road Fabrication
    Replies: 17
    Last Post: 10-10-2011, 08:39 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •