I have my gas flow on 17 , power setting on 2 and wire speed on about 30. When I get in some tight places or other places not convient the puddle hisses and creats little blow holes in the puddle when it cools but can't figure out what is causing it. I have tryed several different settings to no avail. Can someone give me some input on what I'm doing wrong. I feel it's operators error and with the setting but don't know how to adjust eigher. Help.Thanks Mickey