  1. Default IMIG-200 with flux core, running on generator

    Dad snapped the picture so you can not see all the trailers surrounding us or the generator. I fix their golf carts, gator mules, trailers, and more. I need the cash to fix my new truck. Lift tires rims. Normally we haul a couple at a time and weld them. Last trip and this trip we loaded up my truck and did them there and saved a lot of time.

    I am using an IMIG-200 with a porter cable 5500 watt generator and flux core .030. Using flux core since it is outside

    I am posting this since people ask about Everlast MIGs and flux core and generators.

    We do not run the TIGS on generators since they are small generators but the MIG-200 and smaller unit work fine. Plus a TIG would not work well outside and take too long.

    Click image for larger version. 

Name:	c3-mig200genflux.jpg 
Views:	599 
Size:	156.1 KB 
ID:	3988Click image for larger version. 

Name:	2011-08-27-10-22-10.jpg 
Views:	584 
Size:	154.3 KB 
ID:	3987
    Last edited by chadford; 11-10-2011 at 07:02 PM.
    Everlast IMIG-200
    Dad's TIG and plasma
    Lots of tools
    Not lots of space.

Similar Threads

  1. HF Flux Core?
    By Elantramax1 in forum General Welding Questions
    Replies: 7
    Last Post: 10-27-2014, 09:07 PM
  2. Flux Core?
    By Elantramax1 in forum General Welding Questions
    Replies: 57
    Last Post: 09-29-2014, 12:25 PM
  3. Welding with flux core wire
    By Chris A in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 06-08-2014, 05:20 AM
  4. Imig200 flux core welding questions
    By sw2x in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 17
    Last Post: 03-30-2013, 10:24 AM
  5. Gas vs flux core
    By MigPlazArc in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 17
    Last Post: 10-06-2011, 03:11 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •