hey guys, havent been posting much lately, you know what they say, "life happens!!" lol anyway, had a chance last night to get out in the garage and get some more welding practice in.
over the past few months, i've been mostly practicing just laying beads, as jody would say "short arc, long arc, heiliarc in the dark!" just stacking dimes, getting a feel for the footpedal and torch in my hand, ect.
i did a couple projects a while back that came out ok, (a couple sections of aluminum intercooler piping, and some exhaust work) but were very inconsistant as far as bead profile, penetration ect, just because of my lack of seat time.
so, i figured it was time to stop laying beads, and start practicing actual joints.
i hacked up a few peices of 6061-T6 1/8" aluminum, and fabbed up this little thingy..
using the following settings ect:
~99amps footpedal controlled(floored pretty much all the way thruout)
3/32 4043 filler
3/32 yellow tungsten
a/c freq. ~ 100 or so
a/c balance ~ 40%
fitup was pretty poor, i was trying to set it up to weld it as an "outside corner joint" i guess you would call it, but because i cut it out with a 4.5" angle grinder, it was pretty inconsistant, overlapping in some spots.
it the spots where i did get the fitup i was looking for, i was able to get it to keyhole a bit, and was able to get pretty good penetration.
spots where it dont look like the toes are wet in too well is where the crappy fitup came into play.
helpful tips or comments are welcomed, and appreciated! (that means YOU jake, you always give great advice! haha)
on to the pics!
thanks in advance!![]()