MigPlazArc - thanks. I thought the hooks made from mild steel would be the nicest, but figured that I'd need a touch to bend it. I don't have a torch, so I was thinking about plan B.

I had seen the angle on carts other folks had made and thought it looked good. It is a pain to look at, and adjust the PP50 since its on the buttom shelf and not angled. The angle just angles the front so it faces you when your standing and adjust it.

Jason - I think I'll take your advice and put a hook on the underside of the front for the MIG ground cable.