More pictures!Go ahead and critique my welds.
Kinda blowing out still at the end...not leaving an end bead. 6011 at 97 amps Don't know where that seed came from lol
Running to many amps for 6011 rods. Stringer beads. 117 amps
haha got a little welding frost on my shield.
All the rest are 7018 at 117 amps, might be a touch cold. But the slag chipped off in large chunks.
![]()





Go ahead and critique my welds. 
Alex, when you have overstock give me ring!