    Here is a little project I needed to do for a long time.

    It is a trailer mount for a ham radio antenna...Specifically a Texas Bugcatcher antenna. It is a fold over mount that attaches to the ball mount of a trailer hitch.

    I built the mast a while ago and sold the antenna on E-bay. I no longer had the original mount so I had to quickly build the fold over mount this morning so I could ship it out today.

    It is made out of 1/8 plate steel. I used my Powerplasma 50 to cut the metal, my Hobart Handler 210 to tack it up and the Powertig 250 EX to weld it up. Everything went as smooth as can be. Man it sure is nice to be able to cut metal without going through tons of gas or abrasive cut off disks. The Powerplasma 50 cut my cutting time down to almost nothing. I was disappointed that it went so quickly. I was having fun and it went too quick!

    The Powertig 250EX was perfect for welding this up. I did not have to use any tig rods as the fit up was so close as to not have any spacing at all.

    Overall, it took me about an hour to build it. Going to build another sand scoop as a friend wants one after seeing the one I built previously.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_0253.JPG 
Views:	335 
Size:	129.1 KB 
ID:	3245   Click image for larger version. 

Name:	IMG_0252.JPG 
Views:	338 
Size:	136.0 KB 
ID:	3246  
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

Similar Threads

  1. Project 3 from Steve
    By Steve in forum Personal Projects (no welder required)
    Replies: 0
    Last Post: 10-26-2011, 05:33 PM
  2. Project 1 from Steve
    By Steve in forum Hobyist Projects
    Replies: 0
    Last Post: 09-13-2011, 04:33 AM
  3. Steve from Ohio
    By Steve in forum Introduce Yourself
    Replies: 0
    Last Post: 03-02-2011, 07:46 PM
  4. Steve Sims
    By smsims in forum Introduce Yourself
    Replies: 1
    Last Post: 05-15-2009, 06:35 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •