Share
Results 1 to 4 of 4

Thread: Shortened Shifter

  1. #1

    Default Shortened Shifter

    This is a little project I did for my sons car. I shortened his shifter 1 inch for lower profile and quicker shifting. A brand name one would have cost about $150 and eBay about $35 or so.
    First I put Dykem Blue and scribed a reference line down the length. Wasn’t sure if the threads were clocked. Next I took a pipe cutter and cut an inch out of the middle. Then I beveled the edges. Clamped it together and tacked it. A nice little bead and you’re done.
    It was a fun little project to do and saved some money too. The interior is not back in the car so there’s no photo of that yet.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	w14.jpg 
Views:	493 
Size:	52.9 KB 
ID:	40   Click image for larger version. 

Name:	w15.jpg 
Views:	463 
Size:	50.6 KB 
ID:	41  
    POWERMASTER 205 AC/DC Pulse TIG, Plasma and Stick

  2. #2

    Default

    Its a good thing you beveled them. It added valuable strength to the shifter. I may have beveled them a little more to get 100% fusion all the way through.

  3. #3

    Default

    Actually the shifter was only 1/16" hollow tubing not solid. I beveled the full thickness so hopefully I got full penetration. Thanks for for looking out for my interests.
    POWERMASTER 205 AC/DC Pulse TIG, Plasma and Stick

  4. #4

    Default

    It's nice to have the equipment to handle jobs like this. Nice work on the shifter.
    Wayne

Similar Threads

  1. Replies: 9
    Last Post: 03-28-2011, 05:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •