Share
Results 1 to 8 of 8

Thread: Tungsten Question

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Tungsten Question

    When should you use the different sizes, and does it matter?
    1/16
    3/32
    1/8
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  2. #2

    Default

    Amperage, and arc control...That's really somewhat subjective as to what you prefer. Too much heat on too small of tungsten will melt tungsten...Too low of amps with too big of tungsten will eventually allow the arc to wander.

  3. #3

    Default

    I'm having trouble with 1/16 melting a little over time, and 3/32 with the arc wondering. I am running my power arc 140 at 50 amps. The 1/16 tungsten is from Ram Welding supply. Not sure what brand the 3/32 I picked up a couple of pieces from a local machine shop.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  4. #4

    Default

    Sean,
    What mixture are you using? I am using 1.5% Lanth and have not problems at that amperage. Are you using AC or DC? If AC, what is your AC balance. If you are using too much positive time in the balance you most likely will roast your tungsten.
    Lincoln Weld-Pak 100 (C-25 or CO2 Shield)
    Victor Oxy-Act
    Lincoln AC225 Tombstone
    Everlast 250EX & W300 Cooler

  5. #5
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I like the parameters given in the CK Worldwide specs chart:
    http://www.ckworldwide.com/tech-3.pdf

    You can change the grind of your tungsten to make a difference in allowing more heat delivery capacity, or more directional control. It's helpful when you know you are going to run a little hot (or a little cold) for the size of tungsten you have on there.

    For any given diameter tungsten:
    * A "Sharper" tip grind, and/or with less of a flat ground on the end (or even, no flat ground on the end at all, in an extreme case -- leaving the tip "needle sharp") will provide more directional control of the arc/heat.

    * A "Blunter" tip grind, and/or a wider flat ground on the tip will provide more current carrying capacity before the tip melts.

    And certainly the "alloy" of tungsten used can have a huge influence over the current carrying capacity as well. Pure tungsten is lowest, zirconiated one step up, and any of lanthanated/ceriated/thoriated a further step up in terms of current carrying capacity.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  6. #6

    Default

    I'm running 2%(red). I try to use a little more sharper point. I have not played around with a duller point.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  7. #7

    Default

    Yes sizes matter, Check out this website, download the manual and look on page 4 for info on max amps etc for sizes and shape of points http://www.ckworldwide.com/technical.htm

  8. #8

    Default

    I heard that size will also matter depending on the size of your gaps but I was able to fill ~3/8 gap with 1/16 rod by leaving it in the puddle and moving side to side. I have run into the problem where I needed thinner rod for the thickness of the metal I was trying to weld. By the time I could melt the rod, it wanted to burn a hole in the metal.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

Similar Threads

  1. Question on possible tungsten dip contamination.
    By Frank in forum General Welder Questions
    Replies: 6
    Last Post: 06-25-2014, 05:30 PM
  2. Tungsten dressing question
    By Winky in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 06-07-2012, 01:18 AM
  3. Perhaps a silly question about tungsten...
    By Trip59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 05-28-2012, 10:25 PM
  4. Tungsten size question.
    By Brian Ski in forum TIG Welding (GTAW/GTAW-P)
    Replies: 22
    Last Post: 03-25-2012, 07:06 PM
  5. Tungsten grinder question
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 09-06-2011, 05:53 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •