welding direct has them, they are 2.29 each. trouble is you need to place an order of fifty dollars. grainger and mcmaster carr only sell them for1/8th and 1/4 id hose. i had to buy them from this vendor. if i hadn't needed quick connects and another stinger i would have been trying to do something with arc zones female l/h connector to a ???? get the picture. big pain in the axx for a small necessary item.