    I did check that post out and that thread did not answer my question. All I saw was " I think" Or "It looks Like". One guy said he welds old jet engines with them and they seem to work well. I'm not welding jet engines so I was wondering if they are a good thing to have for just everyday fabrication and general welding. Another guy says "HE's heard bad things about them." What in the heck does that mean?" I asked the question "Anyone with EXPERIENCE".....there were a lot of opinions but not much of an answer from those who actually use one.

    One person did say he used one but did not have much experience with tig welding so his opinion was pretty weak.

    I'm looking for someone who is tig fluent and knows what they are doing. I want an opinion on how well those types of cups work from someone who knows welding and uses them.

    I would not have posted if there was a good answer on the site!
    I like clear straight forward answers myself.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  2. #2
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Steve - I guess I would have assumed if someone found a thread on the very topic they were interested in discussing, they would have posted a reply to it, rather than made another, duplicate thread about it.

    Keeping the discussion in one spot makes it easier for others to learn from the topic who happen to search and/or stumble across the thread, no? If everyone made a new thread about every thought they had, the board would become very disorganized and hard for anyone to learn very much about any topic.

    At least, if you posted a link to the other relevant thread in your new thread on same topic, if would help others find the other thread easier.

    Maybe I am in the minority on this philosophy for board organization, though.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  3. #3

    Default

    Quote Originally Posted by jakeru View Post
    Steve - I guess I would have assumed if someone found a thread on the very topic they were interested in discussing, they would have posted a reply to it, rather than made another, duplicate thread about it.

    Keeping the discussion in one spot makes it easier for others to learn from the topic who happen to search and/or stumble across the thread, no? If everyone made a new thread about every thought they had, the board would become very disorganized and hard for anyone to learn very much about any topic.

    At least, if you posted a link to the other relevant thread in your new thread on same topic, if would help others find the other thread easier.

    Maybe I am in the minority on this philosophy for board organization, though.
    Agreed that I should have posted the link. Some folks won't reply to older threads because they feel it is old....but they may have some very good information that was not given before.

    I hear folks say that the topic is old...and it is.
    I am a member of several groups that interest me. For the most part, there is nothing new under the sun anywhere on them. The same questions and comments are made. Sort of like watching a movie for the 10th time. You've seen it and know how it ends, but you still watch as you get a little more detail about the movie in your mind. Sometimes you may even say to yourself, gee, I never noticed that before!

    Usually the only time something really new is offered, it is because there is a new product.

    So there may very well be weldors out there with experience with the clear cups who just got onto this site and maybe they have some relevant information about them. But seeing how there hasn't been a reply....maybe not.

    Just my opinion!
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

  4. #4

    Default

    I agree that this should have gone in the old thread and I think I even replied in it. Since that thread, I took the option of not trying these after reading that people had problems with them but since then I have found people on a different forum that seem to really like them and had no issues using them. Some of them are hobbiest welders and some do it for a living.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  5. #5
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Its all a matter of personal likes and opinions. If someone did not like them then they would have gone away by now.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  6. #6

    Default

    Quote Originally Posted by Tritium View Post
    Its all a matter of personal likes and opinions. If someone did not like them then they would have gone away by now.

    Thurmond
    I wouldn't say that as it would take everyone not to like them and that is slim to none. As mentioned above, someone said they would rather have larger stick out than use one of these and thats not the first time I have heard that so its obvious some people do not like them. Does anyone have an opinion on how well they hold up? I have heard questionable remarks to that also.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  7. #7
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Are there any advantages to using the pyrex cups? Has anyone used these types of cups and found them better than standard cups? I would worry about the cup braking.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  8. #8

    Default

    Quote Originally Posted by DVA View Post
    Are there any advantages to using the pyrex cups? Has anyone used these types of cups and found them better than standard cups? I would worry about the cup braking.
    well one CLEAR advantage (did ya get that pun there ) is that the lens is clean and you have better visability of your puddle. really it all comes down to, can you weld with it, and do you like it. alot of welding is just being comfortable, body position, and how you like your equiptment.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  9. #9
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    I think it is like 49.99 for 10 that is not a bad price but it would be better if it came with a sorted size.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

Similar Threads

  1. Almost a good experience.
    By HoverED in forum Pre-sales, Sales and Shipping questions
    Replies: 17
    Last Post: 09-26-2013, 03:26 PM
  2. Experience with 17 torch and superflex cable?
    By Scetoaux in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 08-08-2013, 04:05 AM
  3. my experience
    By john_electro in forum Introduce Yourself
    Replies: 3
    Last Post: 07-23-2013, 04:49 AM
  4. What's the deal with clear tig cups?
    By ncsugrad2006 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 05-22-2012, 01:50 AM
  5. clear gas cups
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 04-29-2011, 11:16 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •