There is no such thing as repair panels for the lower corners of a 1932 ford trunk lid. I had to come up with my own without changing the shape of the trunk. I have one side finished and the other side half done. I had to make inner and outer patches on both sides





 
					
					 
							
						 Project 2 from Revkev6: 1932 ford Trunk lid repair
 Project 2 from Revkev6: 1932 ford Trunk lid repair
		







 
				
				
				