Share
Results 1 to 19 of 19

Thread: Tig Finger

  1. #1

    Default Tig Finger

    Jody Collier, owner of WeldingTipsandTricks.com has a product that I think is well worth the money.

    It's called a TIG finger. You slip it over your welding glove and it allows you to slide your pinky over the hot metal allowing for a more precise, steady weld without the pain of cooking your finger.

    I have two of them and I can say that it really helps with most all types of welding. I've used it for gas welding, tig welding and mig welding.

    Check it out at http://www.weldingtipsandtricks.com/...tigfinger.html

    Jody has done some reviews of the Everlast equipment and watching his videos will give you some insight on how to set up Everlast tig welders.

    I don't work for Everlast, WeldingTipsandTricks and do not own stock in those companies.

  2. #2
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    They are great Steve. There has been discussion of them in several threads here in the past.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  3. #3

    Default

    As Tritium mentioned, there is already a thread on these. I do think they are nice to have and have used mine a lot. I have also burnt my TIG glove to my finder a couple of times lol. I do find that they can be bulky but that is probably because of the size of my hands.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  4. #4

    Default

    Jason,
    I use the Tig finger and mine has streched out and is very comfortable now. I took the plunge and ordered a three pack. Keep the guide finger from getting toasty.
    Lincoln Weld-Pak 100 (C-25 or CO2 Shield)
    Victor Oxy-Act
    Lincoln AC225 Tombstone
    Everlast 250EX & W300 Cooler

  5. #5
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    I took the plunge and bought the 3 pak, glad I did. More than once, I have had all 3 of them on on at once in certain situations. It's amazing what a difference you can get in control when you have that little extra insulation to allow you to get closer to the weld. Yes, they are bulky, but you will get used to it, and spoiled by not cooking your fingers
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  6. #6

    Default

    Quote Originally Posted by bigjoeinkg View Post
    Jason,
    I use the Tig finger and mine has streched out and is very comfortable now. I took the plunge and ordered a three pack. Keep the guide finger from getting toasty.
    Mine are opposite I need some smaller ones but regardless they do work. I have toasted my TIG fingers though and one of them is discolored now.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  7. #7

    Default

    Heat treated braided fiberglass sleeve can be purchased in 1/4" to 1 1/2" dia. Click image for larger version. 

Name:	14[2].jpg 
Views:	725 
Size:	24.9 KB 
ID:	3199
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. #8
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    How about that- it's about $8 a foot at McMaster...
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  9. #9

    Default

    Yeah you probably can get the basic part cheaper, but I feel that Jody Collier does a great job at Weldingtipsandtricks.com and should be supported. He is a weldor's college degree for free via internet video.

    His Tigfinger is one of the ways he supports the bandwidth and production costs. Buying a few things from him helps keep him making videos and answering questions. I don't know of too many folks with as much welding knowledge as Jody.
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

  10. #10

    Default

    Quote Originally Posted by Steve View Post
    Yeah you probably can get the basic part cheaper, but I feel that Jody Collier does a great job at Weldingtipsandtricks.com and should be supported. He is a weldor's college degree for free via internet video.

    His Tigfinger is one of the ways he supports the bandwidth and production costs. Buying a few things from him helps keep him making videos and answering questions. I don't know of too many folks with as much welding knowledge as Jody.
    I fully agree that Weldingtipsandtricks is a great asset to the welding community, I love his videos and his straight forward no BS approach. He even teaches people to save money where they can. The majority will always buy tig fingers from Mr. Collier, for the few who need a different size or something cheaper, there are alternatives. As for band width and production costs, a youtube channel with that much traffic will turn a healthy profit through AdSense.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  11. #11
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Steve has duplicated yet another thread, which would have been more appropriate for his review:
    http://www.everlastgenerators.com/fo...om-Jody-s-Site

    Please search before you post, guys, and try to help keep information well organized on the board. Anyone trying to research the topic will be much better off, being able to find more condensed information in fewer threads, rather than spread out across many (essentially duplicated) threads.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  12. #12

    Default

    Threads can be merged, but I agree that it's best to keep the board well organized.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  13. #13

    Default

    When I seen them in his videos, I thought to myself that I could easily make those for cheaper but I still ordered a 3 pack, The reason was to support him with the little that I did for his time making those videos and allowing us to watch them and learn for free. It was my way to say "thanks and I appreciate the videos you have made".
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  14. #14
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    I "BUY" his videos on disk also. It is the least I can do to support his good work.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  15. #15

    Default

    Quote Originally Posted by jakeru View Post
    Steve has duplicated yet another thread, which would have been more appropriate for his review:
    http://www.everlastgenerators.com/fo...om-Jody-s-Site

    Please search before you post, guys, and try to help keep information well organized on the board. Anyone trying to research the topic will be much better off, being able to find more condensed information in fewer threads, rather than spread out across many (essentially duplicated) threads.
    I'm not a neat freak. I like a messy desk. I can find a needle in a haystack. But I will admit that I do have a lot of socks with missing other halves. Not sure why socks give me so much trouble...... With that being said.......and not to be argumentative.......

    That is what Google and the advanced search option on this site is for if you want to stay organized. But If I was to post on an older thread, I would get chastised for opening up an old thread. Had that happen so many times with so many other sites. Not just to me but others as well. I don't read posts older than a few months old. Like reading yesterdays newspaper. Old news if you ask me. You just can't win with anyone, anywhere, anymore!

    Just my opinion of course!

    There is nothing new under the sun....even here on this site. Except announcements for new contests and new machines......I really like those.
    Last edited by Steve; 09-12-2011 at 05:35 AM.
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

  16. #16

    Default

    I ordered the 3 pack cause I'm guaranteed to loose at least one. Not only are they good for tig welding, but can be quiet handy when you are torching something out.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  17. #17

    Default

    Quote Originally Posted by welderdude View Post
    I ordered the 3 pack cause I'm guaranteed to loose at least one. Not only are they good for tig welding, but can be quiet handy when you are torching something out.
    The main reason I got 3 was to give one to a friend and I could also use them on more than one finger if desired.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  18. #18

    Default

    so does anyone use these for other welding activities other then just tig? i often find myself running a long bead of flux core and with 1/16" wire, i burn my hands alot. sometimes i like to try to rest my hand on the material and steady myself, this seems like it could help.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  19. #19
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Quote Originally Posted by jerky View Post
    so does anyone use these for other welding activities other then just tig? i often find myself running a long bead of flux core and with 1/16" wire, i burn my hands alot. sometimes i like to try to rest my hand on the material and steady myself, this seems like it could help.
    Yes.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

Similar Threads

  1. Give 'em the finger
    By Rambozo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 10-01-2012, 06:42 AM
  2. Finger-controlled tig torch
    By johnnyfive in forum Pre-sales, Sales and Shipping questions
    Replies: 4
    Last Post: 06-11-2012, 06:14 PM
  3. finger control
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-06-2012, 02:05 AM
  4. 2T/4T Finger Switch for new Torch?
    By Dublin in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 03-26-2012, 03:11 AM
  5. TIG Finger from Jody's Site
    By Gary in forum General Welder Questions
    Replies: 36
    Last Post: 06-02-2011, 02:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •