    I was attempting to weld some 16g tube today and I always hit it with a flap disk and wipe clean with acetone on the outside, but I noticed that I was having one hell of a time because of the contaminants on the inside of the tube where getting pulled up to the surface.

    I didn't really have much probs with not cleaning the inside of the tube when welding
    .120 tube, but the thinner stuff was popping and spewing.

    What is your prefered method to cleaning the inside of a tube before welding? or do you even bother?

  2. Default

    I've never done this kind of welding.
    What I typically hear people doing when tube welding is to back-purge it with argon.

    Go about 3/5 of the way down on this page and you will see a simple Y adapter for back purge and how he set it up with the tube. You will want to seal the argon inlet reasonably well, but leave a little hole in the other end/ends so that the argon can push the air out.
    http://ls1tech.com/forums/cadillac-c...ictures-3.html


  3. Default

    I'm aware of back purging when welding SS, but i'm only welding mild steel.

    The reason I ask is I have seen people tig weld exhaust tube with nothing more than using a wire wheel on the outside and I've also seen people clean it good enough to eat off of... both with seemingly equal results. I, on the other hand not so good of results.

  4. #4
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Cleaning the inside of the tubing (or back side of the weld joint) is important if you will be fully penetrating. That is usually the case with a butt welded joint on .065" thick tubing.

    The main thing is to get any hydrocarbons off of there. Some solvent soaked into a paper towel can work, if the edge of the tubing isn't so ragged that it will cut the towel into bits. If it does have burrs, some deburring can be useful. There are little tools that can make quick work of deburring. I have a tungsten carbide scraper blade I just grab and use in my hands. It never needs sharpening. If you have new tubing, (especially mandrel bent pieces) it may have some oil from being manufactured. Possibly even a thick, wax type coating, which some heat and/or solvents can remove. To clean deep into a tube section, I like to wad a cloth rag into a ball, grab it with one of those flexible long reach type tools, solvent soak it, and run it in and out of the tubing.

    Used exhaust tubing may have corrosion, soot, etc. To remove heavy scale you can use something like a Die grinder with a cartridge roll, cross buff, or flapper stick, followed by a solvent wash, if you want to get the inside really clean. If you don't have a die grinder, but have patience and some good ol' "elbow grease", a strip of emery cloth (sandpaper with cloth backing that comes in a roll...) over your finger can remove stuff. Follow up with a solvent wash. I find solvent in a spray can to be highly convenient sometimes. Can blow the solvent out with compressed air, or wipe it away with a paper towel or rag.

    A cup or end brush that is sized to fit inside the tubing is yet another method.

    If you weld on rusty steel, galvanized or other coated mild steel, don't breathe the fumes, and expect some live popping while welding. Take off any gas lens and use a regular collet body to save you gas lens screens.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  5. #5

    Default

    Remember to never use chlorinated or fluorinated solvents like carb/brake cleaner or 1,1,1 tri...
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. Default

    Lots of good info, thanks!

Similar Threads

  1. But welding sheet metal
    By Ron66 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 20
    Last Post: 09-14-2013, 07:12 PM
  2. Filler metal selection for welding mild steel and 4130 tube
    By hooda in forum General Welding Questions
    Replies: 11
    Last Post: 03-21-2013, 07:38 PM
  3. Need some tips on welding sheet metal to 3/8 plate
    By Haywire in forum Stick Welding (SMAW)
    Replies: 13
    Last Post: 06-07-2011, 03:56 AM
  4. Welding on Galvanized metal
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 5
    Last Post: 04-04-2011, 08:32 AM
  5. Tungsten Sharpening.. Cool method..
    By sschefer in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 11-14-2010, 03:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •