Hello,
I recently got the PU205 unit, I've used a mig machine for a couple of years mostly making misc repairs or making custom tools and figured I could probably pick up tig fairly easy.
Not the case so far... i'm kind of stumped. First off, my settings are...
3/32 red tungsten
7-10 Lpm pure Argon
played around with 6 and 7 cups
60-70amps on 1/8" mild steel ground down to shiney
Ive tried finger and pedal
I think thats everything...
At first I used acetone to meticulously clean the tungsten and metal before welding, but I don't think that made a difference really. The problem i'm having is an intermittent one. At times I can get a decent arc and other times the arc gets soo bright and flickers that I can't see anything.
I suspect it might be argon gas flow related, but i'm not sure?? Ive tried turning up the argon to 15lpg just to see if there is a difference and I still have the same problem. I weld in a closed garage and even made sure to keep the machine away from the work so that the fan won't disturb the argon when welding.
Every once in a while, about 3 out of 10 tries I can get a nice smooth arc and puddle going. So far I havn't even been able to get to the point of trying filler rod yet.
I'm starting to get pretty frustrated because Ive studied up for about 6months now and felt like ive taken all of the right steps to tig, but I can't even get a simple puddle going most of the time...
What do you guys suggest?