  1. #1

    Default Changing gas to Mig Aluminum

    I am looking for an easy way to be able to switch from 75 /25 to Argon when I mig Aluminum, the Argon is hooked to my tig and both share the same cart. Id love to see pictures and get a description of your setup. I hate the thought of doing the hose clamp thing.

  2. #2

    Default

    A Y valve from Western will work. About 50.00. Available through almost any welding supply store. Simple to hook up and use. Need two regulators though.
    http://cgi.ebay.com/Western-Y-Connec...-/170477454504

  3. #3
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Sounds like you could use a compressed air, quick disconnect fitting. To switch the gas, you'd need to just unplug one gas hose, and plug in another. Readily available, inexpensive... (Would need a flowmeter/regulator on each gas bottle.)
    '13 Everlast 255EXT
    '07 Everlast Super200P

  4. #4

    Default

    I did what jakeru did and used 1/4" quick disconnect fittings on my 2 regulators. Its a pretty slick way of doing it.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  5. #5

    Default

    I HIGHLY discourage the use of quick connectors...Why? Because the sudden depressurization will introduce moisture into the lines. It'll collect around the mouth of the fittings and go unnoticed and will be introduced as things are coupled and decoupled. Stick with a static fitting setup with less movement. Open and shut a valve and that's it. Also quick couplers have a nasty way of interfering with flow consistency and accuracy as the spring on ball connections can offer variations of degrees of opening. Automotive types, tend to wear and leak over time, with many repeated cycles.
    Last edited by performance; 08-11-2011 at 10:18 PM.

  6. #6

    Default

    Quote Originally Posted by performance View Post
    I HIGHLY discourage the use of quick connectors...Why? Because the sudden depressurization will introduce moisture into the lines. It'll collect around the mouth of the fittings and go unnoticed and will be introduced as things are coupled and decoupled. Stick with a static fitting setup with less movement. Open and shut a valve and that's it. Also quick couplers have a nasty way of interfering with flow consistency and accuracy as the spring on ball connections can offer variations of degrees of opening. Automotive types, tend to wear and leak over time, with many repeated cycles.

    I am pretty sure they are referring to using the quick disconnects on the outlets of the regulators (low pressure side), and still using two regulators.

    Not sure how it would be much different from the quick connector on the front of my 200DX tig, or different from pulling a hose off of a barb and re-attaching.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. Changing to a gas lens what do I need.
    By PeterA in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 11-09-2012, 05:56 PM
  2. Project #3 from DVA: Stool for changing brakes
    By DVA in forum Other Custom Fabrications
    Replies: 7
    Last Post: 10-19-2011, 04:19 AM
  3. Replies: 2
    Last Post: 08-03-2011, 03:50 PM
  4. changing settings while welding
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 04-05-2011, 01:36 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •