Thread: more torch questions

  1. #1

    Default more torch questions

    I ordered 25' torch with my PP256. The welder showed up with the standard blue handled 15' wp18 torch. This is the euro style torch and it's quite big.

    The 25' torch arrived a couple of days later. It is marked SR20 , which I imagine correlates to WP 20. It is similar in size to a wp9 air cooled, so nice and compact, just like the torches in Mark's recent post. As Mark said there would be, it has a switch on it. This is just a little plastic switch zap strapped on. At first I planned to remove the switch in order to make the torch a bit less bulky, however I find the switch provides a good finger grip on top when the torch is held from underneath like a pencil.

    Also. the switch can come in handy now and then for tacking things in difficult spots. So it'll stay for now.

    I might put a short piece of large heat shrink on the torch handle to outer sheath connection. Right now that is done with electrical tape, that looks like it won't last very long.

    What is the amperage rating for this small torch (with cooler in use)?

    This is a rigid torch and there was no flex neck in the package. Is a flex neck available for this torch?

    Glen
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  2. #2
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Glen, My airgas catalog list the Model 20 as a 250 Amp water cooled torch.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  3. #3

    Default

    That makes sense Thurmond, it was sent out to go with the 250 amp machine.

    Hopefully a flex neck is available for it, that would be ideal for my usage.

    I can't see a need to ever use the larger wp 18 watercooled torch that came in the box.

    Glen
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  4. #4
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Glen, That 18 series is 350 Amp. I think the handle that holds the switch comes off leaving a normal smaller sized handle beneath. I have seen a Chinese seller on e-bay that has VERY low priced heads. Usually under $20 or so delivered. I have ordered plasma consumables from them and I got them in 1 week flat. On the downside though they advertised the consumables as genuine Trafimet which they weren't and got their auctions for those items pulled by e-bay.

    Thurmond
    Last edited by Tritium; 08-07-2011 at 10:41 PM.
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  5. #5

    Default

    thanks Thurmond, I'll check that seller out.

    Glen
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

Similar Threads

  1. Torch questions
    By DJLVA in forum Pre-sales, Sales and Shipping questions
    Replies: 11
    Last Post: 07-10-2017, 12:07 AM
  2. Different torch questions
    By Gunther in forum Pre-sales, Sales and Shipping questions
    Replies: 6
    Last Post: 07-05-2017, 10:10 PM
  3. Model 26 Torch & General Torch Questions...
    By Ray C in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 08-26-2012, 04:47 PM
  4. torch type questions
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 03-31-2011, 08:14 AM
  5. Torch hand control questions
    By hammerbait in forum General Welder Questions
    Replies: 10
    Last Post: 08-07-2010, 01:29 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •