Share
Results 1 to 2 of 2

Thread: Aluminum Boat Fuel Tank Support Structure (jakeru's #?)

  1. #1
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default Aluminum Boat Fuel Tank Support Structure (jakeru's #?)

    [edit: this is jakeru's project #18[

    I welded a fuel tank support into the hull of an aluminum boat, and a structure to raise the deck above it up higher, to provide room for the top of the tank.
    Click image for larger version. 

Name:	IMG_0007_fitting_together.jpg 
Views:	576 
Size:	139.1 KB 
ID:	2999

    Here are the welds on the actual fuel tank support, down low in the hull of the boat. I used the torch switch at I think somewhere in the area of 180-190 amps, with 1-2 seconds of post-flow to feather the heat down where needed. Went through quite a few sticks of 1/8" 5356 filler rod on this.
    Click image for larger version. 

Name:	IMG_0026_fuel_tank_support_rear_piece.jpg 
Views:	557 
Size:	131.9 KB 
ID:	3005 Click image for larger version. 

Name:	IMG_0027_fuel_tank_support_stern_piece_2.jpg 
Views:	586 
Size:	136.6 KB 
ID:	3003
    C-clamps were useful for jigging up the pieces.
    Click image for larger version. 

Name:	IMG_0029_fuel_tank_support.jpg 
Views:	555 
Size:	134.6 KB 
ID:	3004

    I cut some pieces with the horizontal bandsaw (It's a natural for cutting tubing/bar stock, such as this)
    Click image for larger version. 

Name:	IMG_0001_bandsaw_cutting.jpg 
Views:	566 
Size:	145.4 KB 
ID:	3002

    Other tools I made use of are, a 4.5" angle grinder with a flap wheel (for removing paint to prepare surfaces for welding) and also a nonferrous grinding wheel (for removing material, to fine-tune the fitment of the pieces.)

    Sometimes you get creative with methods to clamp, pre-stress, and hold pieces in just the right position to get those tack welds on there. Here I used a claw-hammer and two C-clamps to pry and hold a piece into position for tack welding with both hands free (to manipulate TIG torch and filler rod.)
    Click image for larger version. 

Name:	IMG_0008_pry.jpg 
Views:	539 
Size:	138.2 KB 
ID:	3001

    It was kind of tricky getting good vision in some spots, while crawling around in the boat hull doing this work. Sometimes I feel like I really could use a welding helmet that is tighter to my head. (How annoying is it when you think you can see, are all ready to weld, flip the helmet down and "bump" goes the helmet - hey I can't see!) This was on a fishing boat I had done some work welding work on before.
    Click image for larger version. 

Name:	IMG_0013_floor_support.jpg 
Views:	568 
Size:	134.7 KB 
ID:	3000

    A lot of this extruded aluminum alloy was 6061. When welding 6061 to 6061, it's important to provide a space for filler rod to be added into, to dilute the puddle and avoid hot cracking. You can see I beveled the edge of some rectangular (6061) tubing where some (6061) angle would be stitch welded to it. I did not want to build up a tall raised bead, because this structure needed a flat surface to support a deck above it.
    Click image for larger version. 

Name:	IMG_0009_clamped_and_beveled.jpg 
Views:	593 
Size:	135.2 KB 
ID:	3008

    Here is how those top surfaces turned out:
    Click image for larger version. 

Name:	IMG_0020_starboard.jpg 
Views:	593 
Size:	137.4 KB 
ID:	3006 Click image for larger version. 

Name:	IMG_0017_weld_bead.jpg 
Views:	563 
Size:	128.9 KB 
ID:	3009

    (continued next post due to 10 picture per post limitation...)
    Last edited by jakeru; 07-29-2011 at 12:50 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  2. #2
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I wanted to get in a few more pictures that wouldn't fit in the first post...
    Click image for larger version. 

Name:	IMG_0015_port.jpg 
Views:	553 
Size:	139.7 KB 
ID:	3012
    The piece labeled "no weld" is removable (tight-fitting in its slot) for being able to access the fuel tank below.

    This section in the bow was tricky to weld with the torch switch, thin wall it had to be welded to, etc. But, think it will hold?
    Click image for larger version. 

Name:	IMG_0042_front_piece.jpg 
Views:	528 
Size:	140.3 KB 
ID:	3011

    Overall shot
    Click image for larger version. 

Name:	IMG_0039_overall.jpg 
Views:	565 
Size:	141.7 KB 
ID:	3010
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. Aluminum Cartop Boat Transom Gussets (jakeru's #16)
    By jakeru in forum Welding Repairs
    Replies: 4
    Last Post: 01-20-2012, 02:23 PM
  2. Replies: 2
    Last Post: 08-03-2011, 03:50 PM
  3. Aluminum diamond plate flooring, for a fishing boat (jakeru's #10)
    By jakeru in forum Other Custom Fabrications
    Replies: 5
    Last Post: 07-15-2011, 03:19 PM
  4. Custom Harley Fuel Tank (jakeru's #11)
    By jakeru in forum On Road Fabrication
    Replies: 0
    Last Post: 07-06-2011, 08:41 AM
  5. Aluminum Boat Fishing Rod Mounting Plates (jakeru's #8)
    By jakeru in forum Other Custom Fabrications
    Replies: 6
    Last Post: 06-28-2011, 09:10 AM