A friend had a small 6x7 trailer and wanted to add a foot to the back. Nothing fancy and took a couple hours. Did it after that sword I posted. It was a pop-up camper and we flipped the axle for him to. The picture makes the U bolts look crooked but they are not. Bent the side channe; parts on the brake and use angle for the rest. Will not go on the road it for building to carry a water tank and presure washer. Done with IMIG-200.

before and axle flipped
Click image for larger version. 

Name:	imagejpeg_2_2.jpg 
Views:	540 
Size:	119.4 KB 
ID:	2983

Added bent channel
Click image for larger version. 

Name:	imagejpeg_2_4.jpg 
Views:	552 
Size:	114.5 KB 
ID:	2981

Done added some middle support to
Click image for larger version. 

Name:	imagejpeg_2_3.jpg 
Views:	549 
Size:	129.9 KB 
ID:	2982