    Default Project 15 from d3javoodoo % Aluminum Wheel repair #2 %

    This morning I took an hour out to begin some repair work for a set of wheels I got for free years ago from a friend who runs his own machine shop.



    Click image for larger version. 

Name:	IMG_0001.jpg 
Views:	475 
Size:	135.4 KB 
ID:	3063



    I have decided these will make a good set if I put a little elbow grease into it...


    Click image for larger version. 

Name:	IMG_0002.jpg 
Views:	498 
Size:	143.6 KB 
ID:	3060 Click image for larger version. 

Name:	IMG_0004.jpg 
Views:	470 
Size:	142.4 KB 
ID:	3061

    You can see from the above photos that the tapped holes are not centered correctly on this one individual wheel...

    Click image for larger version. 

Name:	IMG_0011.jpg 
Views:	508 
Size:	145.7 KB 
ID:	3064 Click image for larger version. 

Name:	IMG_0012.jpg 
Views:	523 
Size:	147.4 KB 
ID:	3065

    The cure I came up with was to add some weld, & then grind off excess, then polish, & or sandblast ...
    I didn't take the time to get that stack of nickels look because all that excess meat will be ground off... but I was sure to achieve good fusion. These wheels currently are 4" x 2.25" x 1/4" well thickness (aluminum). I plan to set aside @ least 5 hours in the future to make these wheels look GOOD.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_0003.jpg 
Views:	419 
Size:	142.8 KB 
ID:	3062  
    As a man thinketh, so shall he be.

Similar Threads

  1. Aluminum wheel crack repair
    By jakeru in forum Welding Repairs
    Replies: 8
    Last Post: 06-18-2013, 10:46 PM
  2. Using Helium for Aluminum Wheel Repair (jakeru's #19)
    By jakeru in forum Welding Repairs
    Replies: 16
    Last Post: 02-18-2012, 04:29 AM
  3. Project 7 from d3javoodoo ^custom wheel design^
    By Legacyartist247 in forum Other Custom Fabrications
    Replies: 2
    Last Post: 07-30-2011, 06:31 AM
  4. Project 12 from d3javoodoo ^ Jig for sm. Scale Wheel (5 spoke) ^
    By Legacyartist247 in forum Hobyist Projects
    Replies: 0
    Last Post: 07-27-2011, 03:46 AM
  5. Project 6 from d3javoodoo * Alloy wheel repair*
    By Legacyartist247 in forum Welding Repairs
    Replies: 5
    Last Post: 07-21-2011, 03:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •