    Well awhile back I made a temp catch can out of left over exhaust pipe that I had sitting around. I finally got to order the parts to make my proper can and spent a day to do it. Materials consisted of 3" 6061 pipe, 3/4" 6063 pipe, SS wool sponges, 4043 Filler, 6061 12AN bungs, SS braided PTFE line 12AN, 12AN fittings. Tools were press, 4 1/2 grinder, welder, drill and bit.

    Materials


    Cut the small piece open and flattened it on my press. Then cut off corners with angle grinder and then made them round. You can see one on top of the pipe.


    After the top and bottom were completed, I welded on the bottom and then used some more of the extra small pipe to make an inner section to hold the SS wool.


    The fitting was welded on the side for now but I will do it different later.


    Here is the can with wool


    Welded shut with nipple on top for the filter.


    The fitting is located as I showed above. The plan is to cut it off later and make a flat angled section to and weld it into the pipe and the fitting on it.

    Total time was maybe a couple of hours. It did not take too long really but I did not keep track as I was doing 3 other things in the mix of this.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  2. #2

    Default

    hmm I am not seeing any of the pics
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  3. #3

    Default

    Quote Originally Posted by dgarnier View Post
    hmm I am not seeing any of the pics
    I wonder if the host was down at this time. They are loading for me fine right now.. Let me know.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

Similar Threads

  1. Replies: 2
    Last Post: 01-07-2013, 07:10 AM
  2. Anyone who makes Aluminum catch cans or reservoirs...Question?
    By CGCINC in forum General Welding Questions
    Replies: 9
    Last Post: 12-08-2011, 01:38 PM
  3. Project 14 from Jason: Scout
    By Jason in forum Welding Repairs
    Replies: 10
    Last Post: 07-31-2011, 05:48 AM
  4. Project #5 from Jason: Exhaust #2.
    By Jason in forum On Road Fabrication
    Replies: 2
    Last Post: 06-13-2011, 05:56 AM
  5. Aluminum catch cans
    By dlong in forum Other Custom Fabrications
    Replies: 4
    Last Post: 07-11-2010, 11:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •