Share
Results 1 to 3 of 3

Thread: Project 7 from d3javoodoo ^custom wheel design^

  1. #1

    Default Project 7 from d3javoodoo ^custom wheel design^

    Here are a few pics of another project of mine that I've been working on ... For a while now I've had some ideas in relation to automobile design in every aspect. Recently though I have began to lay the groundwork for a (custom) rolling chassis to support multiple small scale concept vehicle designs.
    Click image for larger version. 

Name:	IMG_0181.jpg 
Views:	582 
Size:	141.3 KB 
ID:	2884 Click image for larger version. 

Name:	IMG_0180.jpg 
Views:	609 
Size:	142.6 KB 
ID:	2883

    these are images of a single wheel design currently in progress. I choose to use 1/4" x x1/2" crst stock to begin fabrication of the bulk of the spokes, & plastic pipe section for the center wheel well. Eventually when the original is complete I'll make a mold to reproduce in different mediums like plastic, aluminum, bronze, etc.
    As a man thinketh, so shall he be.

  2. #2

    Default Recent pics...

    Here are a few updated photos of this 6 spoke design, which may or may not be used for the next model..

    Click image for larger version. 

Name:	IMG_0257.jpg 
Views:	598 
Size:	141.7 KB 
ID:	2987 Click image for larger version. 

Name:	IMG_0309.jpg 
Views:	583 
Size:	142.7 KB 
ID:	2988


    Click image for larger version. 

Name:	IMG_0310.jpg 
Views:	575 
Size:	142.3 KB 
ID:	2989 Click image for larger version. 

Name:	IMG_0324.jpg 
Views:	602 
Size:	143.1 KB 
ID:	2990otos
    As a man thinketh, so shall he be.

  3. #3

    Default A labor of love...

    Well this afternoon after that hot sun went down, I got a little work done.

    Click image for larger version. 

Name:	IMG_0037.jpg 
Views:	598 
Size:	144.5 KB 
ID:	3025

    I'm a few steps closer to a rolling chassis...

    Click image for larger version. 

Name:	IMG_0038.jpg 
Views:	566 
Size:	143.5 KB 
ID:	3026 Click image for larger version. 

Name:	IMG_0040.jpg 
Views:	623 
Size:	145.2 KB 
ID:	3027

    @ this point I've chosen to use 1/8" instead of 1/4' to decrease weight.
    As a man thinketh, so shall he be.

Similar Threads

  1. Project 1 from Trip - new cart design (re-run contest)
    By Trip59 in forum Other Custom Fabrications
    Replies: 4
    Last Post: 10-29-2012, 03:35 AM
  2. Project 15 from d3javoodoo % Aluminum Wheel repair #2 %
    By Legacyartist247 in forum Welding Repairs
    Replies: 0
    Last Post: 07-30-2011, 09:43 PM
  3. Project 12 from d3javoodoo ^ Jig for sm. Scale Wheel (5 spoke) ^
    By Legacyartist247 in forum Hobyist Projects
    Replies: 0
    Last Post: 07-27-2011, 03:46 AM
  4. Project 8 from d3javoodoo % Side job%
    By Legacyartist247 in forum Welding Repairs
    Replies: 3
    Last Post: 07-21-2011, 10:23 PM
  5. Project 6 from d3javoodoo * Alloy wheel repair*
    By Legacyartist247 in forum Welding Repairs
    Replies: 5
    Last Post: 07-21-2011, 03:46 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •