    Here is a splitter I made for my larger top mount intercooler:

    I made it from a sheet of metal from lowes, I think it was either 16gauge or 18 guage sheet metal. Also to bend the pieces, i made a quick sheet metal brake. And to make the holes, i found a socket that fit inside of another socket and just drilled a hole and set up the sockets and hammered them together to make a dimpled hole.








  2. #2

    Default

    Also to make a seal against the intercooler, I used this seal from mcmaster.com

    http://www.mcmaster.com/#bulb-seals/=d91mut

    its the edge grip seal number 1 i forget what size but it does a great job with the sealer and i found it helps to make the pieces in cardboard first
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  3. #3
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Thanks for the link on the mcmaster carr rubber seals!

    I've had times I've wanted to get some more of this type of material for projects, but had no source, or even known how to search for it. "edge grip seal" and "bulb seal"... who'da thunk it!

    PS - nice job on the intercooler ambient air baffles
    '13 Everlast 255EXT
    '07 Everlast Super200P

  4. #4

    Default

    Haha yeah I must have searched for days or even weeks for some sort of material to use. Mcmaster has pretty much everything youll ever need so its a great source for when you need any sort of hardware. And thanks i want to put a middle splitter to separate the air so it cools the intercooler more efficiently but it is cold to touch after driving the way it is now
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

Similar Threads

  1. project 2 from bob wills, dec 3 contest, log splitter for loader
    By bobwills in forum Heavy Equipment and Commercial Projects
    Replies: 9
    Last Post: 04-24-2012, 04:43 AM
  2. Project 2-6 from Hooda-Weld Blowoff valve on intercooler
    By hooda in forum Personal Projects (no welder required)
    Replies: 3
    Last Post: 03-01-2012, 01:58 PM
  3. Project 4 from bobwills- Skid loader log splitter
    By bobwills in forum Heavy Equipment and Commercial Projects
    Replies: 16
    Last Post: 10-12-2011, 04:53 AM
  4. Project 3 from bobwills- log splitter wedge
    By bobwills in forum Other Custom Fabrications
    Replies: 4
    Last Post: 10-08-2011, 05:42 PM
  5. Project #1, from Haywire, a firewood splitter.
    By Haywire in forum Hobyist Projects
    Replies: 0
    Last Post: 06-25-2011, 08:29 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •