    I fabricated a custom waste linkage for a hybrid turbocharger (large compressor wheel, small turbine wheel) in stainless steel.

    I probably had more time in cutting and grinding of the pieces to fit just right (maybe 20 minutes) than I did in the actual welding (10-15 minutes.) I used 304 stainless rod, plus the cut apart pieces of the original wastegate linkage, (which may have been nickel plated steel of some sort, as it was magnetic.)

    I tack welded the linkage with it installed on the turbo (using the welder's finger / third hand for grounding) and actually held the piece with my left hand, as I zapped the first tack autogenously right TIG torch (and plenty of current) in my right hand. It worked like a charm!
    Click image for larger version. 

Name:	linkage_before_welding.jpg 
Views:	523 
Size:	133.0 KB 
ID:	2857 Click image for larger version. 

Name:	tack_welded.jpg 
Views:	524 
Size:	127.3 KB 
ID:	2856

    Then after getting the second tack weld on there, I removed the linkage and welded it up on the benchtop.
    Click image for larger version. 

Name:	welded_front.jpg 
Views:	548 
Size:	140.2 KB 
ID:	2854 Click image for larger version. 

Name:	welded_back.jpg 
Views:	565 
Size:	125.9 KB 
ID:	2855
    I was going for some rainbow coloration in the weld beads, for a fun and kind of a neat "custom welded" look. And I think it turned out that way pretty much. I used a #6 gas lens with about 12 cfh argon. To get the look, I would purposely pull the torch away during the later stages of post-flow. If you held the post flow on there too long, you would have a silver spot where the weld ended. If the heat was just right when you pulled away the torch during post-flow, the area turns a pretty color. (Actually, I've noticed the "oxidation film colors" are actually inverted rainbow colors; the same colors one sees when looking at a thin oil film/slick floating on water.)

    Here is the completed product after being installed back on the turbo:
    Click image for larger version. 

Name:	installed_linkage.jpg 
Views:	525 
Size:	143.8 KB 
ID:	2858 Click image for larger version. 

Name:	completed_overall.jpg 
Views:	526 
Size:	141.6 KB 
ID:	2859

    I used 1/16" 309LSi for the filler rod. 1/16" tungsten with fairly sharp tip (small flat in the end). Low frequency pulsing about 1.5 pulses per second, 60% pulse duty, and 60% background. Footpedal for current control. (Turned way up quite a bit for the first tack welds, then turned down to about 2/3rds of tack weld setting for the full welding.)

    Before I welded this, I was welding some mild steel on another project and was having problems on arc starting (arc would try to start back up near the collet body, before moving down to tungsten tip.) For this project I had all of the shielding gas flow related parameters the same, the only adjustment I made was a slight increase in pre-flow. And it was only a very small change in the pre-flow setting... like increased from .5 second to .6 second. It however made all the difference in helping the arc start smoothly.
    Last edited by jakeru; 07-16-2011 at 11:46 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  2. #2

    Default

    Looks beefy! You might considered titanium next time if you like funky blue colors.... titaniums been known to do so.*****
    As a man thinketh, so shall he be.

  3. #3

    Default

    That looks sweet, how much boost are you planning on running and what is the turbo going on?
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  4. #4
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I've got no plans for it; except for just wanting it out out my shop, and I decided to make it functional before putting it up for sale. At one point I was considering importing turbos as a side business, and this was one of the samples I got. Its part number matched perfectly what I ordered, but the rest of the turbo was completely different and not what I expected.

    I figured it might be actually marketable now that the wastegate is actually functional (no longer just a "kit of parts", as it was when I received it.)

    Interested in it? Contact me via IM; I'm open to offers. (Save a bundle over buying a name brand turbo!)

    Also, I've got one other new turbo "sample" that needs to go (will be selling it as well); it's smaller than this one. So if anyone is looking for a turbo for their project, let me know! Thanks.
    Last edited by jakeru; 07-18-2011 at 02:00 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  5. #5

    Default

    Sorry I dont want it i just recently purchased a Borg Warner Turbo for my car but maybe someone else on here will want it, good luck and nice fabrication
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

Similar Threads

  1. Stainless Steel oxy-acetilene welding, how-to?
    By lwmar in forum General Welding Questions
    Replies: 7
    Last Post: 10-06-2011, 05:12 AM
  2. Racing Kayak Rudder Linkage (stainless steel TIG - jakeru's #20)
    By jakeru in forum Other Custom Fabrications
    Replies: 0
    Last Post: 08-01-2011, 04:20 AM
  3. Custom Toyota 4-cylinder Intake Manifold (jakeru's #17)
    By jakeru in forum On Road Fabrication
    Replies: 9
    Last Post: 07-31-2011, 12:50 PM
  4. Custom Harley Fuel Tank (jakeru's #11)
    By jakeru in forum On Road Fabrication
    Replies: 0
    Last Post: 07-06-2011, 08:41 AM
  5. Stainless Steel Stick Welding?
    By Oxide00 in forum General Welding Questions
    Replies: 13
    Last Post: 04-27-2011, 02:31 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •