Thread: Press for the brake. $35 total, that was for the jack.

  1. Default Press for the brake. $35 total, that was for the jack.

    Here are some pictures of the press. The middle bottom and frame. Not sure what order they are in cause I can not figure out upload.

    Top of frame
    Click image for larger version. 

Name:	2011-07-04-12-25-46.jpg 
Views:	461 
Size:	161.0 KB 
ID:	2690
    base shelf
    Click image for larger version. 

Name:	2011-07-04-12-26-03.jpg 
Views:	504 
Size:	152.5 KB 
ID:	2689
    Spring locations
    Click image for larger version. 

Name:	2011-07-04-12-42-49.jpg 
Views:	504 
Size:	150.7 KB 
ID:	2688
    Complete no sanding no paint but can use it
    Click image for larger version. 

Name:	2011-07-04-13-09-25.jpg 
Views:	507 
Size:	150.2 KB 
ID:	2687
    Brake added
    Click image for larger version. 

Name:	2011-07-04-17-37-19.jpg 
Views:	508 
Size:	147.9 KB 
ID:	2686
    1/4" piece bent, did 1/2 to and it cracked
    Click image for larger version. 

Name:	2011-07-04-18-05-50.jpg 
Views:	474 
Size:	153.1 KB 
ID:	2685
    Click image for larger version. 

Name:	2011-07-04-12-25-16.jpg 
Views:	504 
Size:	147.9 KB 
ID:	2691
    Middle for jack before welding. They are no in order sorry
    Click image for larger version. 

Name:	2011-07-04-12-24-48.jpg 
Views:	475 
Size:	152.1 KB 
ID:	2692

  2. Default

    Well it got paint yesterday. Could not pick a color. Took hunter green and sunny yellow. A lot of yellow. Match the welders now. lol

    Added a place for jack handle
    Click image for larger version. 

Name:	2011-07-09-19-44-16.jpg 
Views:	501 
Size:	152.7 KB 
ID:	2778

    Used rustoleum
    Click image for larger version. 

Name:	2011-07-09-14-25-40.jpg 
Views:	490 
Size:	161.5 KB 
ID:	2779

  3. Default

    All done.

    Click image for larger version. 

Name:	2011-07-10-08-35-38.jpg 
Views:	516 
Size:	166.2 KB 
ID:	2780

  4. Default

    The handles on the sides were bent on the press with the brake I made too

  5. #5

    Default

    Nice! What is the largest width you can bend? I would love to build one that could bend 3'-4' pieces of 12 gauge.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  6. Default

    So far 1/2" by 2 I have done with no problem. Last post I did in the brake thread was 6"x1/4" with no problem either. It is pretty strong.

  7. #7

    Default

    Your projects look good, whats next on your build list?

  8. Default

    Scooter,

    I fixed a clamp for my Dad last night. A cheap plastic Harbor Freight one now steel on one end. Will post picture in a second.

  9. Default

    Oh yea I will be fixing a poolman's trailer tonight will try to get picture.

  10. #10

    Default

    Where did you get the jack at Harbor Freight? I can deffinately see this on my build list very soon
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  11. Default

    The jack is from Harbor Freight. Itwas $34.95 on sale.

    Poolman backed out but welded a 22' trailer tounge last night. Will try and to get pictures today. Not much work just to stop it from rattling.

Similar Threads

  1. Press brake for modified HF shop press
    By Scooter in forum Other Custom Fabrications
    Replies: 18
    Last Post: 06-06-2011, 07:29 AM
  2. Press brake
    By Ram48 in forum Other Custom Fabrications
    Replies: 34
    Last Post: 03-28-2011, 02:55 PM
  3. See user Total Distorsions pictures at pirate4x4
    By admin in forum Customer Testimonials
    Replies: 1
    Last Post: 08-05-2009, 12:08 AM
  4. A link to Total Distortsion's Everlast post
    By admin in forum Introduce Yourself
    Replies: 0
    Last Post: 06-08-2009, 10:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •