A local shop agreed to supply me with their drops for welding practice. I go get a bucketful, weld them together and then go back and exchange them for more drops. I don't have to pay for practice material and their drops come back heavier. Not much of a gain for them, they're really just doing me a favor.
Anyway.. they're cutting circles out of 1/4" plate on their plasma table for a customer. The foreman suggested that I weld the small ones onto the large ones to get used to welding a curve and holding a consistent rod angle while doing it. I don't know how successful I was, but it's good practice I suppose.
I decided to stop playing around with all the different rods and stick with 7014 till I can get a consistently good bead with that (or I run out of the 5lb I have). Then I'll move on to the others.
Here's what I ended up with.
Attachment 1888Attachment 1889




Reply With Quote