Having some problems with the consumables on the 256. Both with the ones that came with it and the new ones that I bought at the time I purchased the welder. The electrodes average about 28.7mm. When I install the electrode then screw on the tip all the way it will light once then not relight. However if I loosen the tip a turn it will work perfect everytime. This of course tells me the electrode to tip clearance is not sufficient enough and is allowing the electrode to arc directly to the tip and stay attached. So is this a problem with the consumables or a problem with the actual torch itself? I just hate having to leave it loose for it to work properly and don't want to replace the torch with another brand since I already have a large amount of consumables for this one