Re: Everlast CUT60 received for Test
Ok Everlast sent a rolling standoff with their unit. I decided to finally give it a test.
1st Picture shows standoff on 1/4" steel
2nd Picture shows the cut 1/4" steel
3rd Picture shows standoff on 1/2" steel
4th Picture shows the cut 1/2" steel
The rolling standoff maintained a 1/4". I tried to adjust to a standard 1/16-1/8" standoff but found I could not adjust the way it fits. It maintains a fixed standoff of 1/4". I think the cuts would be better if the rolling standoff was fixed at 1/16" or 1/8". I felt the 1/4" was a bit to far from the material to give a real fine quality cut.
Attached Images![]()
![]()
![]()
![]()