    Re: Everlast CUT60 received for Test
    Ok here's some picture's of the unit before it Everlast's send their Prepaid shipping label

    1st frontal picture of the unit you can see just how powerful the cooling fan is.

    2nd the cooling fan intake is huge on this unit

    3rd Notice the heavy duty soldering connections.

    4th top shot photo

    5th side shot photo
    Attached Images
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  2. #2

    Default Specter part 2

    Re: Everlast CUT60 received for Test
    1st Pierce Test Aluminum 1/16, 1/8, 1/4, 5/16, 3/4"

    2nd Cut Aluminum 1/16, 1/8, 1/4, 5/16, 3/4"

    3rd Pierce and Cut Steel 1/4, 3/8, 1/2, 3/4"

    4th Cut Steel 1"

    5th Cut Steel 1 1/4"

    Sorry for the delay in pictures. But I just got that Sony Mini dvd camera back from the repair shop.
    Attached Images

    __________________
    Own farm:Harris oxyacy torch, lincoln 225, stick,Century 135GL mig, Hypertherm PowerMax 45 Plasma Cutter
    Co-Own CNC shop:Miller :1251 plasma cutter, MaxStar 700 TIG/Stick, & XMT 456 Multiprocess Welder.Hypertherm HPR260 Plasma Cutter
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3

    Default Specter Part 3

    Re: Everlast CUT60 received for Test
    Ok Everlast sent a rolling standoff with their unit. I decided to finally give it a test.

    1st Picture shows standoff on 1/4" steel

    2nd Picture shows the cut 1/4" steel

    3rd Picture shows standoff on 1/2" steel

    4th Picture shows the cut 1/2" steel

    The rolling standoff maintained a 1/4". I tried to adjust to a standard 1/16-1/8" standoff but found I could not adjust the way it fits. It maintains a fixed standoff of 1/4". I think the cuts would be better if the rolling standoff was fixed at 1/16" or 1/8". I felt the 1/4" was a bit to far from the material to give a real fine quality cut.
    Attached Images
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Review of my new I-MIG 200.
    By 225 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 9
    Last Post: 03-10-2013, 07:42 PM
  2. Powerarc 140 review
    By atatro in forum Stick Welding (SMAW)
    Replies: 40
    Last Post: 06-13-2012, 01:12 PM
  3. 3 month review
    By mdkrusemark in forum Customer Testimonials
    Replies: 7
    Last Post: 02-12-2011, 08:54 PM
  4. Gerals41 from weldingweb
    By everlastsupport in forum Customer Testimonials
    Replies: 0
    Last Post: 08-05-2009, 02:42 AM
  5. LINK: Everlast TIG work on weldingweb.com
    By everlastsupport in forum Customer Testimonials
    Replies: 2
    Last Post: 08-05-2009, 12:04 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •