    Here is a set of articulated arm clamps I welded up. The material used was 1’ ball bearings, 3/8” plate, and ¾” round stock for the construction. 3/8” bolts to tighten each clamp when in position. I welded up different ends for either clamping to my table or the material I am going to weld. Bolts, Vice grips. And angle iron ends shown in the pictures.

    Have fun
    Tom
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	clamp in action (7) A.jpg 
Views:	487 
Size:	135.1 KB 
ID:	2698   Click image for larger version. 

Name:	ball clamp.JPG 
Views:	457 
Size:	110.6 KB 
ID:	2697   Click image for larger version. 

Name:	clamp in action (6).JPG 
Views:	473 
Size:	142.1 KB 
ID:	2696  

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  2. Default

    i love that, how stiff is it when you tighten the ball joints? you should patent that

  3. Default

    Thats pretty awesome. It's a giant set of helping hands.
    Did you use a lathe to modify the bolts so the bearing would set in the end?

  4. #4
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default

    Quote Originally Posted by parkour View Post
    Thats pretty awesome. It's a giant set of helping hands.
    Did you use a lathe to modify the bolts so the bearing would set in the end?
    I use the Helping Hands to solder wires together, recognizedthem right off. Looks like a really useful tool. I’ve never seen one that big before.


    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  5. #5

    Default

    Very nice. The Giant Helping Hands. If they where on the market I am sure they would sell. I have a smaller set for soldering and a bigger set for circuit boards. Never thought about a set for welding.

    Neat idea Tom.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6

    Default 1" balls

    here is where I bought the balls
    http://www.vxb.com/Merchant2/merchan...e=BearingBalls

    but they are cheaper here
    http://www.mcmaster.com/#9528k33/=d26ur8

    have fun
    tom

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  7. Default

    listen jester i know it seems like its to soon but i want to get married that way you and i and the clamping arms can live happily together

  8. #8

    Default

    I did use a lathe but that could be done with a drill press or even in a vise. just cut the head off and drill the end with a small bit first then go bigger to get the dimple as shown.
    The arm holds very well this picture show one arm holding a 1-1/2" square tube and the black clamp suspended in the air with no other support.

    have fun
    Tom
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	clamp in action (1) A.jpg 
Views:	395 
Size:	129.0 KB 
ID:	2706  

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  9. #9
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default


    Did you get the ball bearings out of a CV joint or something?



    This is too cool, I’d pay money for something like this, ifit wasn’t an arm and a leg$
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •