    Couple of weeks ago I had an issue with the foot pedal. Mike hooked me up with
    some parts and the foot pedal now works.

    Today I used the machine and the post flow wont shut off. (Post flow is set to "0").
    The only way to shut off the argon is to shut the machine down.

    Anyone run into this?

    Thanks

  2. #2

    Default

    This may sound dumb, but will the post flow shut off if you actually set it? 1-2 sec?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. #3
    Join Date
    Jun 2011
    Location
    Charleston, South Carolina
    Posts
    50

    Default

    Tried that, it did the same thing. It does show
    the seconds on the display (but it won't shut off).
    Bottom line the only way to stop the
    flow is to shut the machine off.

    Thanks

  4. #4

    Default

    Brian is being handled via EMAILs. So I will not duplicate the response until it is fixed.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    I had a similar problem with my PU 205 at first. It was just the spring in the gas valve. Alex told me about this. Apparently there were a few machines at that time that had the problem, maybe yours has the same problem.

    I took the valve apart and stretched the spring a little. That fixed it.
    The valve with the stretched spring is still in there a year later , works fine.

    Alex sent me a replacement gas valve but I haven't bothered to put it in because the original one works fine now.

    Glen
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  6. #6

    Default

    So now Brian has been told this twice. Once by Everlast support (via email this morning) and once by a customer that had the same issue over a year ago. I told him it is rare, but I am sure that's the issue.

    We were doing this via email, then it shows up on the forum. This makes more work for us this way.

    He did have other issues as well that are now worked out. Spring should get him going 100%, thanks for the help Worntorn.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. Default

    Quote Originally Posted by brianscott View Post
    Tried that, it did the same thing. It does show
    the seconds on the display (but it won't shut off).
    Bottom line the only way to stop the
    flow is to shut the machine off.

    Thanks
    I am experiencing a similar problem at the moment with my 200DX (about to try stretching the spring again while I wait for a new solenoid to be shipped). One trick I've found other than shutting off the welder entirely is to take the Argon hose between the torch and where it plugs into the welder and bend it over on itself to put a kink in it. When the Ar flow in the meter starts to drop, usually you can release the hose and the back pressure now causes the solenoid to close. Your mileage may vary, but it's a bit more convenient than shutting the welder down after every pass. I'm not sure I'd want to put the hose under that kind of stress for thousands of cycles, but it works for a few times.

Similar Threads

  1. Another "issue" with gas flow
    By JohnT in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 04-30-2018, 08:11 PM
  2. Everlast Super200P died. Performed "diode-ectomy". Now it's welding again!
    By jakeru in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 18
    Last Post: 01-27-2015, 09:24 PM
  3. Northern Industrial 1644910 AD Helmet Opinions? (3.82" x 2.44" view area)
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-10-2013, 03:49 PM
  4. Replies: 11
    Last Post: 10-30-2012, 06:43 PM
  5. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •