The first photo shows the 1/4" thick piece being cut to shape. The third and fourth photos show the completed bracket after welding and grinding the front edge round.
Next I milled a short piece of 1" thick round SS to form the stand blade. This fits into the bracket as shown in the last photo.




Reply With Quote