Share
Results 1 to 2 of 2

Thread: aws weld cert G6 open root

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Jun 2011
    Location
    flordia tampa
    Posts
    16
    Blog Entries
    1

    Default aws weld cert G6 open root

    has anybody done this test with power pro 205.Not with inspector but at home .i did test with mig .035 down for root then pulse mig .035 up for cover & cap for high pressure freon tanks. would like to do one test tig root up then stick 7018 fill/cover up.then do test all tig weld up

  2. #2
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    have you got your 6010 root 7018 hot n cover in 6g yet ? normally that is gone after first then the tig root 7018 hot n covers then full tig root out
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

Similar Threads

  1. tig root 2G lay wire technique?
    By GaveUpOnTV in forum General Welding Questions
    Replies: 7
    Last Post: 08-08-2016, 01:30 PM
  2. 2" sch 80 tig root 7018 cap 6g test help
    By Boilermech in forum General Welding Questions
    Replies: 26
    Last Post: 05-03-2013, 05:25 AM
  3. School project from Jerky (3g tig root)
    By jerky in forum Hobyist Projects
    Replies: 7
    Last Post: 02-20-2012, 04:23 PM
  4. Open to all suggestions
    By Nikola Tesla in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 03-13-2011, 08:22 PM

Posting Permissions