Share
Results 1 to 4 of 4

Thread: Horse Stall Door Sign

  1. #1

    Default Horse Stall Door Sign

    Made from 16 GA. carbon steel. Took somewhere around 3 hours drawing time and 24 minutes to cut. Cut on a my home-built 50"x96" CNC plasma table using the PP50.
    Althought slightly warped due to the heat and thin material, it was kept to a minumum by spraying it with water while cutting. (No water table... yet)

    The size is 36" wide x 24" high.

    The horses name is Rolex. His racing name is Grand Halo, and the parents names are below.

    Click image for larger version. 

Name:	emmc_100MEDIA95IMAG0550.jpg 
Views:	473 
Size:	134.5 KB 
ID:	2642

  2. #2

    Default

    That looks sharp! Do you have any pics of your plasma table?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. #3

    Default

    Very nice. I envy you. CNC is on my list, but a long way away for me. Nice size machine you have.

    Like to see table pictures as well if you have any.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    Here are a couple pictures I have. I need to figure out how to get the others off my phone. Most of the material was free and laying around, so I made it with what i could get. Now that I can cut out precision parts, I'm starting to redesign and upgrade the table.

    Click image for larger version. 

Name:	IMAG0220.jpg 
Views:	442 
Size:	144.8 KB 
ID:	2707 Click image for larger version. 

Name:	IMAG0227.jpg 
Views:	441 
Size:	144.3 KB 
ID:	2708
    Click image for larger version. 

Name:	IMAG0231.jpg 
Views:	441 
Size:	146.3 KB 
ID:	2709 Click image for larger version. 

Name:	IMAG0228.jpg 
Views:	423 
Size:	141.7 KB 
ID:	2710
    Click image for larger version. 

Name:	IMAG0224.jpg 
Views:	426 
Size:	146.2 KB 
ID:	2711 Click image for larger version. 

Name:	IMAG0223.jpg 
Views:	479 
Size:	145.0 KB 
ID:	2712
    Click image for larger version. 

Name:	IMAG0226.jpg 
Views:	467 
Size:	146.4 KB 
ID:	2713 Click image for larger version. 

Name:	IMAG0229.jpg 
Views:	447 
Size:	146.1 KB 
ID:	2714
    Click image for larger version. 

Name:	IMAG0230.jpg 
Views:	457 
Size:	144.6 KB 
ID:	2715 Click image for larger version. 

Name:	Render-1.jpg 
Views:	460 
Size:	8.7 KB 
ID:	2717

Similar Threads

  1. Al Horse trailer
    By robt in forum General Welding Questions
    Replies: 3
    Last Post: 03-01-2015, 07:48 PM
  2. Sign for the Forward Township Athletic Association
    By cpierce18 in forum Personal Projects (no welder required)
    Replies: 10
    Last Post: 04-30-2013, 05:49 PM
  3. Project 2 from CGCINC: Category: Aluminum outdoor sign
    By CGCINC in forum Hobyist Projects
    Replies: 9
    Last Post: 06-13-2012, 02:05 AM
  4. Cart before the horse
    By footboarder in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 02-22-2011, 03:26 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •