    Here is an adapter I made for my new tig torch. I bought a WP-26 torch from Ebay with gas through the lead but no dinse connecter. I had a round brass bar so I machined an adapter. I machined a 1/8” threaded port in the side of the adapter for the gas supply. . I removed the dinse connecter from my Everlast stick stinger and used it with the adapter to connect to my PM-256.

    Have fun
    tom
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	gas connecter for tig (1).jpg 
Views:	750 
Size:	145.9 KB 
ID:	2611   Click image for larger version. 

Name:	gas connecter for tig (5).jpg 
Views:	739 
Size:	98.9 KB 
ID:	2612   Click image for larger version. 

Name:	gas connecter for tig (4).JPG 
Views:	668 
Size:	144.3 KB 
ID:	2613  

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  2. #2
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Hey Tom, I am not using the dinse connector you sent me on the 26 series torch (it doesn't fit anything I have either). I will send it back to you if you can make me one of those adapters (don't mind paying you for the machine work of course). I don't need the protrusion for the dinse connector to attach to the adapter. I will just drill and tap a hole where the protrusion would have been to hook up a lead from my solar panel.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  3. #3

    Default

    Here be another one for tritium
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	adapter for tritium (1).jpg 
Views:	677 
Size:	131.1 KB 
ID:	2643  
    Last edited by acourtjester; 07-02-2011 at 10:05 PM. Reason: spilling

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  4. #4
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Sweet, Tom. Perfect. I PM'd you as well.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

Similar Threads

  1. Adapter for weld tec
    By Steves1967 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 01-06-2018, 04:37 PM
  2. Everlast MTS 200 1 lb. Spool Adapter
    By jheggie in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 04-08-2015, 06:34 PM
  3. dinse adapter for 210ext
    By miker2 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 11-06-2012, 03:39 AM
  4. tig torch options and dinse connector adapter 3/8 size.
    By rab in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 02-12-2012, 05:16 PM
  5. PowerArc used with Tig power adapter??
    By Oxide00 in forum Stick Welding (SMAW)
    Replies: 8
    Last Post: 06-06-2011, 07:44 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •