To back Mark up here, I have never had a call with someone not plugging in the MIG torch (in fact MIG calls are VERY rare). I have had few calls on which port to plug it into, but rare and it is in the manual.
Also, you should straighten your regulator up, the tube with the ball inside should be vertical. Otherwise you are going to waste your gas.
I was a little confused when I heard no spark, but saw welds on the steel in the pictures. Anyway. Hope you are up and running now. Mark asked you a couple times. And like Mark said, the manuals are updated/improved through-out the year and as we add/change features, so it is always recommended to download the manual.
I just bought an O-scope, I had read the manual before I even ordered the product.