Well I have not used the plasma part of my power pro 256 until tonight I hooked it up and gave it a try. Usually we just grab the torch or a smaller parker plasma if we need. Since I have not used mine before I figured I would give it a try and ran into some problems. I had it set at 35A then 50A and 60PSI and 80PSI line pressure to cut 3/16 plate. I figured between those settings something should cut this like butter but was denied. In my frustration to get it working I decided that I would take the guide off and I finally got it to cut by pulling the trigger, tapping the tip to the metal and then pulling it back up a tad. If I did not tap it down it would not blow through. At 35A it hardly left a gouge and at 50A it went maybe half way through..

Now when I got the machine I had weird issues with it not starting up correctly(made a buzzing sound and had an orange? light on).. This went away after turning on and off the machine 3 or 4 times. I did notice that with the stock TIG torch I had a hard time getting the arc to start but also had something funny with the torch going on. I hooked up a WP20 and only had maybe 2 bad arc starts or so..

My question is, does this sound like its the points or sound like the machine is having a problem some place. I opened it up and did not see anything really wrong in my quick glance. I couldn't locate a set of filler gauges to check the points so I will have to purchase a set here soon.