    Just wanted to post a couple of pictures of the only project I have had these last 6 years. I'm still not finished but I'm far enough along to share. It's real exciting to be at this stage. Any way, here she is after paint. Just took off all the masking paper today.





    The tail end is black so it's a little hard to see. Some parts still need to be installed and wheel covers need to be fit up.



    edit to add: I posted this in the no welder required section but I actually did a little welding. I drilled two holes in a steel bracket in the wrong spot. A little tig weld to close it up and re-drill was needed.
    Last edited by RV8guy; 06-25-2011 at 12:31 AM.