So here is a little project that called my attention. When the owner was attempting to change brakes, a lug bolt stripped out and would not budge. I tried everything that I could to get this out and finally came up with a simple solution. Time spent was a couple hours of fighting.
First new rotor/hub
So the start of this was put a lug extractor on it... Should get it out... NOPE.. I was putting all my strength into it when I heard SNAP.. Thinking sweet I got it to break out of there.... NOPE.... Split my new lug extractor down the side... Craftsmen so it got replaced. Problem is I broke one and didn't get it to budge so I didn't want to snap yet another..
I decided I would try a chisel to break the head and No go as I assumed. Then I proceeded to drill it out with the expectation it would fail and sure enough I had enough after not long.. That left it here
I decided since I did not have access to an oxy-ace at this time, I would simply pull the hub and caliper and wheel and everything else at once and then finish the brakes. After I would get the wheel free..
Brakes done
My plan of attack now it drill through the old hub and relieve the lug bolt.
I drilled just until I hit the wheel..
and off..
Next time, I will just pull the wheel off all together and go at it this way again if the extractor breaks. A brand new lug bolt was used in place of destroyed one. Tools were drill, drill bit, hammer, extractor, sockets, ratchet and chisel...













Reply With Quote
)
You are right that the only damage to remain was the 2 spots it hit the wheel. Those spots are maybe a dimple if that. I pretty much hit surface and quit. It was crazy how well those 2 wholes worked. After drilling the wholes, I was able to unthread the bolt with a socket hardly grabbing it. I always thread lug bolt in by hand with a socket only and then I pull out the torque wrench to finish them off. I am not sure that this was just over torques but think that maybe they cross-threaded it. Like I said, I could not budge it with a 3 foot fence poll on my breaker bar. I can get the front axle nuts off with just a breaker bar and they are at 195ft/lbs.

I've broken my share of midrange quality easy-outs over the years.