  1. #10

    Default

    Quote Originally Posted by Jason View Post
    It looks like that flux works really well. I am gonna have to pick some up to try out for my next stainless projects. Anyone compare the flux to back purging? Is it cheaper to use one verse the other?
    I just did a ton of stainless exhaust tubing for a set of custom headers. The fit up was pretty poor and there was a ton, I mean a TON of welding to be done on them. they were constructed from an assortment of mandrel bent pieces by the fab guy at our shop. Basically he just cut a bunch of pie slices out of the various pieces of tubing to get the general shapes down and brought it to me for welding. With the long pieces I was back purging with pure argon but that is much harder to do with a two or three inch piece because of the heat generated. I went and bought some solar flux and let me tell you that stuff is awesome. It burns black when you weld over but seems to sand out ok.. It is cheaper and easier welding than back purging, but if you are filling big gaps like I was and the flux gets to the topside of the weld it makes it a little difficult to tell where the flux is and where the base metal is. the flux will melt and puddle and accept filler just like the base metal so you have to really make sure to get the heat in there. But IMO overall the flux is better and less problematic than back gassing. I also had to weld the inside of some of the joints which isnt possible when purging. I got a one pound can at local LWS for about 40$. It was totally worth it if you dont already have a spare bottle and regulator or a dual regulator.
    Last edited by Wrenchtamer; 06-19-2011 at 01:47 PM.
    Everlast PP256
    Everlast Imig 205
    HF 90 am inverter tig
    Scopes, Scanners, Meters

Similar Threads

  1. SS Exhaust pipe weld settings? (PowerTig 225LX)
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 12-27-2011, 12:33 AM
  2. Harley exhaust (crossover pipe?) TIG welded
    By jakeru in forum On Road Fabrication
    Replies: 0
    Last Post: 11-10-2011, 07:57 AM
  3. Project # 4_ yotarover _ exhaust straight pipe
    By yotarover in forum On Road Fabrication
    Replies: 9
    Last Post: 06-11-2011, 09:15 PM
  4. Replies: 0
    Last Post: 04-29-2011, 06:41 AM
  5. Stainless exhaust pipe
    By dchatcher in forum General Welding Questions
    Replies: 13
    Last Post: 03-09-2011, 06:44 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •