    The mosquito whine Ogorir is probably what your used to then. But More inductance results in better wetting in.You've probably welded with units with low inductance, like Miller. I am used to ESAB. Here's what a weld looks like at the level I described. Low inductance as you recommend leaves a tale tale ridge in the middle.Attachment 2532Attachment 2530Attachment 2531