Quote Originally Posted by dgarnier View Post
Would it weld to the back side?
Nope. Copper is often used as a back-up material. Best to find somehting fairly thick though as this sheet will not work. Also, copper will conduct the heat fairly quickly, this can be good or bad, depending on the situation.