This is project 6, from dgarnier, Fillin' holes
Reworking the Fan Mount on my bow fishing rig and I had 4 3/8" holes to fill in on some 3/16 plate. Since its been out in the weather its pretty rusty so I wire brushed it to clean it up as best I could, but it was still not too clean. So I opted for some 6011 1/8 rod to fill in the holes. Well I had to use some sort of backer, So I just used some scrap steel, looking back this was mistake 1. I think I would have been better off with some brick or something. The scrap got welded to the bottom of the plate, nothing a hammer couldnt fix but not the best way about it. Mistake 2 was not putting enough weld metal on top of hole so I ended up having to fill in a bit more.
Attachment 2448
Attachment 2451
This time I hit it with the wire wheel and switched to tig and just worked around the hole dabbing in filler and filled the hole. Then a little clean up with the grinder and some paint after it cools down and it will be good to go back on the boat.
Attachment 2449
Attachment 2450
sold my miller mig
got a PT250EX
saving up for a plasma cutter