    Default Project 2, from Tritium, Tractor Seat Stool

    This is my second project, a stool made from an old metal tractor seat and post and a tandem plow disk.

    Attachment 2410Attachment 2411Attachment 2412

    Step 1 was to cut a hole in the disk for the seat post with my Everlast PU 205P Multi-Process set up as a plasma cutter.

    Step 2 was to cut 2 pieces of 3/4" by 2" steel the width of the seat post to reinforce the junction of the post to the disk.

    The plasma cutter handled both the thin disk and the thick steel very nicely.

    Step 3 was to MIG weld the reinforcements to the seat post leaving a stub below to pass through the square hole in the disk.

    Step 4 was to tack weld the seat post and reinforcements to the disk and check the alignment.

    Step 5 was to complete the welding to the disk with my MIG (.30 flux core wire used)

    Step 6 was to heat the stool post with a torch and bend it to center the seat over the center hole of the disk (this also leveled the seat to the perfect height and shifted the center of gravity to the sweet spot)

    Step 7 is in process and involves painting with Green Rustolium paint.

    A finished pic will follow after the paint job is done.

    Materials used: 1 old tractor seat and post, 1 old tandem plow disk, 2 pieces of 3/4" thick steel 2" by 3", Green Rustoleum Paint.

    Estimated time for completion including painting and drying. 24 hours.

    Thurmond
    Last edited by Tritium; 06-14-2011 at 03:38 AM. Reason: changed title to comply with contest rules
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  2. #2

    Default

    Hey do you have any more tracktor seats laying around I would like to make one of those seat myself.
    Looks cool.

    have fun
    Tom

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  3. #3
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    I will look around my metal stockpile. I might have one.
    You can get one here though: http://www.tractorsupply.com/tractor...r-seat-0237681

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  4. #4

    Default

    Thanks for the link I had looked on Ebay back a few months ago for one but all the had was high priced one from old tractors.
    They were priced for age not function. We just got a tractor supply here in town I will check it out.

    have fun
    tom

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

Similar Threads

  1. 2013 summer project #1 - Shop stool
    By youngnstudly in forum Hobyist Projects
    Replies: 5
    Last Post: 08-07-2013, 06:15 PM
  2. Project 1 from Tritium, Welding Cart.
    By Tritium in forum Personal Projects (no welder required)
    Replies: 3
    Last Post: 01-07-2012, 08:12 PM
  3. Project #3 from DVA: Stool for changing brakes
    By DVA in forum Other Custom Fabrications
    Replies: 7
    Last Post: 10-19-2011, 04:19 AM
  4. Project 3, Solar Tig Welding, from Tritium
    By Tritium in forum Hobyist Projects
    Replies: 5
    Last Post: 06-22-2011, 12:48 AM
  5. Project 1, Third Hand, from Tritium
    By Tritium in forum Other Custom Fabrications
    Replies: 0
    Last Post: 06-13-2011, 09:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •