I received my Everlast LX 225 welder a few days ago and have an issue with
the foot pedal. It has a reverse effect when using. If I set the amps on the panel at 50A as soon as I start the machine with the foot pedal the amps jump to 100A then will rise with more foot pedal then go back down with full foot pedal.
The following are reading with different amp settings:
Amps Start foot pedal 1/2 foot pedal full foot pedal
8 100 amps 140 amps 10 amps
50 100 amps 150 amps 63 amps
100 100 amps 170 amps 101 amps
150 109 amps 175 amps 164 amps
What I dont understand is if I set Amps on the machine at 100 how could the foot pedal go higher than 100.
Anyone have this problem (The trigger on the torch works fine)
Thanks
Brian