Share
Results 1 to 12 of 12

Thread: Problem with foot pedal on LX 225

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Jun 2011
    Location
    Charleston, South Carolina
    Posts
    50

    Default Problem with foot pedal on LX 225

    I received my Everlast LX 225 welder a few days ago and have an issue with
    the foot pedal. It has a reverse effect when using. If I set the amps on the panel at 50A as soon as I start the machine with the foot pedal the amps jump to 100A then will rise with more foot pedal then go back down with full foot pedal.

    The following are reading with different amp settings:



    Amps Start foot pedal 1/2 foot pedal full foot pedal
    8 100 amps 140 amps 10 amps
    50 100 amps 150 amps 63 amps
    100 100 amps 170 amps 101 amps
    150 109 amps 175 amps 164 amps

    What I dont understand is if I set Amps on the machine at 100 how could the foot pedal go higher than 100.

    Anyone have this problem (The trigger on the torch works fine)

    Thanks

    Brian

  2. #2

    Default

    Turn your upslope off. Are you using it in 2T?

  3. #3
    Join Date
    Jun 2011
    Location
    Charleston, South Carolina
    Posts
    50

    Default

    Yes. Upslope in off and using 2t.

  4. #4

    Default

    Has the rack slipped on the pinion? I had this happen the other day. The result was a bit different than you are experiencing though.

    On my pedal, the rack moved away from the pinion on the return stroke. The result was it only turned the pinion part way back to it's zero position. Now with the pedal fully up, the pinion is turned to where it should be with the pedal pushed part way down, so the starting amps are higher than they should be. This kept happening until the foot off the pedal starting amps were so high that I could not control the puddle.

    By flexing the rack away from the pinion I rolled the pinion back to it's proper starting location against the internal stop on the POT. A little tweaking of the rack and tightening of the holding screw got things working properly again.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  5. #5

    Default

    I got your message, but could not make out the number. Ray or Mike though would be best to answer this question. Its possibly a bad pot.

  6. Default

    Brian,
    You ever get your foot pedal working right?

    I'm having problems with my 225 foot pedal and curious about different solutions.
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

  7. #7
    Join Date
    Jun 2011
    Location
    Charleston, South Carolina
    Posts
    50

    Default

    Foot pedal Problem is now fixed! Works like a champ.

    Mike sent me a (4053) chip, couple of diodes and a capacitor.
    Replaced the parts and now the (Herman Monster) foot pedal works properly.

    Brian

  8. Default

    Gee, I never looked at the read-out while I was welding so I don't know what the amps are. One thing is, when I try to start, it will buzz. Then when I look at the read-out it will usually say 13 or 14 amps and won't fire til the amps read what I dialed it to. It's a little different than your issue. I kinda thought it was normal to have to wait for the TIG to 'catch up'. Is your's doing anything like that??
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

Similar Threads

  1. Powerpro 205 tig pedal problem
    By toxicturtle in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 05-20-2016, 01:59 PM
  2. Poweritig 200 foot pedal problem
    By Gunny10r in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 11-06-2014, 04:22 PM
  3. powerpro 256 pedal problem ?
    By cdale2002 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 05-30-2014, 04:42 AM
  4. foot pedal problem
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-17-2010, 03:06 PM
  5. superultra 205 foot pedal problem
    By agrrob in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 10-31-2010, 11:42 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •