Share
Results 1 to 5 of 5

Thread: DIY Tig Electrode sharpener

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default DIY Tig Electrode sharpener

    Here is a sharpener I made for the tig electrodes. It’s a HF trim router with a 2” sandinh disc. Works great, sharpening at the 6 and 12 oclock positions cuts straight lines on the electrode. check out youtube video
    http://www.youtube.com/watch?v=D7a5HQQxISA

    Have fun
    Tom

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  2. #2

    Default

    I like that setup! I need to get away from using my angle grinder! Did you have to do anything for the sanding disk to fit the router?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. #3

    Default

    No the router and the disc shaft are both 1/4" I used 120 grit. Its a roloc 3m disc.
    The base is a 1/4" plate with a "U" shaped clamp to hold the router it has a small on/off switch in it's end.
    The electrode holder has different size holes for different size electrodes.

    hav fun
    Tom

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  4. Default

    Sharpening the tungsten eats the grinding wheel pretty fast for me (compared to how steel would have). How is the sanding disk holding up? Some people talk about using a diamond blade.

  5. #5

    Default

    I have not had to replace the disc yet and I think it will hold up for a good amount of time.
    I did try a dimond blade but the grit was too rough and ate the tungston up to quickly. I'm sure finer grit is out there but I wanted a smaller diameter to be able to do shorter electrodes.

    have fun
    Tom

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

Similar Threads

  1. $39 Harbor Freight tungsten sharpener
    By DaveBonds in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 14
    Last Post: 03-22-2014, 01:35 PM
  2. chemical tungsten sharpener
    By bubbas55 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 11-09-2012, 02:21 AM
  3. Electrode
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 03-31-2012, 04:28 PM
  4. tungsten sharpener
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 34
    Last Post: 12-28-2011, 12:43 AM
  5. Really Cheap $19.98 Tungsten Sharpener
    By JohnS in forum TIG Welding (GTAW/GTAW-P)
    Replies: 34
    Last Post: 04-21-2011, 05:36 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •